Order grout for a bond beam lintel, not concrete. Pick it in this order: grout type, strength, slump, specification method, and admixture rules. The drawings and the project specification control every number on this page.
What does a bond beam lintel get filled with?
A bond beam lintel gets grout that complies with ASTM C476, the standard specification for grout for masonry. Grout is a fluid cementitious mixture of cement, aggregate, optional lime, and enough water to flow into the cells around the reinforcement.
Concrete and grout differ in how they are placed. Concrete goes into non-absorptive forms at a lower water content. Grout goes into absorptive masonry units at a high slump, and the units pull excess water out as it hardens. That is why the mix that leaves the truck looks wetter than ordinary concrete: the water that the units will absorb is part of the design.
Fine grout or coarse grout?
ASTM C476 defines two types. Fine grout uses sand smaller than 3/8 in. as its only aggregate. Coarse grout adds pea gravel smaller than 1/2 in. alongside the sand. Aggregates for either type follow ASTM C404.
Choose by the geometry of the grout space first. The governing factors are the minimum clear dimensions of the space, the grout pour height, and construction economics. Coarse grout is typically more economical to produce.
A workable field rule: clear grout spaces of 2 to 3 in. or less, or a minimum clearance of only 1/4 in. between the reinforcing bar and the unit, call for fine grout. Larger spaces with more than 1/2 in. of clearance around the bars generally take coarse grout. Pour height also affects the choice, so check it with the drawings.
A bond beam lintel course in a typical 8, 10, or 12 in. wall usually has enough channel width for coarse grout. A narrow channel block or tight bar clearances change the answer to fine grout.
What strength does the grout need?
When grout is specified by strength, the minimum is 2,000 psi at 28 days, tested per ASTM C1019. Project requirements can call for a higher strength.
Under the unit strength method, the Specification for Masonry Structures (TMS 602) requires the grout compressive strength to equal or exceed the specified masonry strength f'm, but never below 2,000 psi. For strength design of concrete masonry, a maximum specified grout strength of 5,000 psi applies; that cap limits the specified value, not the field-tested result.
As an economic rule of thumb, CMHA recommends balancing the specified grout strength with the specified masonry assembly strength, so that one element of the system does not end up considerably stronger than the other.
What slump does the grout need?
ASTM C476 requires a grout slump of 8 to 11 in., measured by ASTM C143. The slump must let the grout flow into the smallest grout spaces and around obstructions such as reinforcing bars, anchors, and mortar fins.
Choose the end of the band from the conditions. An 8 to 9 in. slump suits damper weather, low-absorption units, wider grout spaces, and shorter lifts. A 10 to 11 in. slump suits drier weather, high-absorption units, narrower spaces, and taller pours.
Do not cut the water to make a stiffer grout on the theory that it will be stronger. The high initial water content compensates for absorption by the masonry, and the units remove much of it during and after placement. Studies cited by CMHA show adequate grout compressive and bond strengths from high-slump grout placed in masonry units.
How is the grout specified: by proportion or by strength?
ASTM C476 allows two routes. The proportion route mixes to the Table 1 volume proportions. The strength route sets proportions from 28-day compressive strength tests that meet or exceed the specified strength. Written acceptance of the grout mix submittal is required before grouting operations start.
The Table 1 boundaries are: fine grout, 1 part portland or blended cement, 0 to 1/10 part hydrated lime or lime putty, and 2-1/4 to 3 times the sum of the cementitious-material volumes of fine aggregate. Coarse grout uses the same cement, lime, and fine-aggregate band, plus 1 to 2 times the sum of the cementitious-material volumes of coarse aggregate.
A site-mix check uses bulk densities from ASTM C476: portland cement 94 lb per ft3, hydrated lime 40 lb per ft3, damp loose sand 80 lb per ft3. Take 1 ft3 of cement with 2.75 ft3 of sand and no lime. The sand is 2.75 times the cementitious volume, which sits inside the 2.25 to 3 band, so the batch complies with Table 1. Converted to weight, the dry batch is 94 lb of cement plus 220 lb of sand, 314 lb in total. Raise the sand to 3.5 ft3 and the batch breaks the maximum: 3.5 times the cementitious volume is outside the proportion spec, so either reduce the sand or use the strength method.
With the strength route, an accredited testing laboratory and the grout producer establish the proportions, and the mix design lists what meets the specifier's requirements. That route can also give better structural compatibility with the specified masonry units, since proportion-table mixes often test well above the minimum.
What admixture and mixing rules apply?
Admixtures must appear in the project documents or be approved by the purchaser. ASTM C476 prohibits antifreeze compounds used to lower the freezing point of grout. Admixtures containing chlorides should not be used in grout: chlorides can corrode the embedded steel and contribute to efflorescence in the wall. Air-entraining materials are not recommended where the grout bonds to reinforcing bars.
Site-mixed grout needs at least 5 minutes in a mechanical mixer with enough water to reach the desired consistency. If water is added at the site, remix for at least 1 minute before discharging. Ready-mixed grout may also have its slump adjusted at the site to the desired consistency. Hand mixing is acceptable only for small volumes and only when the specifier approves it.
How do you check the batch ticket?
Match these lines on the ticket to the submittal and the specification before grouting starts: design strength in psi at or above the drawing minimum; grout type, fine or coarse, matching the approved submittal; slump of 8 to 11 in. at placement; cement, lime, and aggregate proportions inside the Table 1 bands or matching the tested mix design; and admixtures limited to those the purchaser approved.
| Check | Source value | What fails it |
|---|---|---|
| Grout type | Fine or coarse per ASTM C476 | Coarse grout in a channel too narrow to pass the bars |
| Strength | 2,000 psi minimum; drawing value governs | Ticket strength below the drawing minimum |
| Slump at placement | 8 to 11 in. per ASTM C143 | Low slump in a tall, narrow pour that needs flow |
| Proportions | ASTM C476 Table 1 bands or tested mix design | Site batch with sand outside the 2.25 to 3 band |
| Admixtures | Only purchaser-approved products | Chlorides, antifreeze compounds, or unapproved additions |
| Submittal status | Written acceptance before grouting starts | Grouting begins with an unapproved mix |
Common grout mix mistakes on bond beam lintels
- Ordering concrete instead of grout for the lintel course.
- Using fine grout in a wide bond beam channel, where coarse grout does the same job at lower cost.
- Ordering coarse grout for a narrow channel where the stone cannot pass the reinforcement.
- Cutting water to stiffen the grout, which starves the flow around the bars.
- Adding water at the site without the required remix time.
- Judging grout strength from cylinders cast in non-absorptive molds, which does not represent grout hardened inside absorptive masonry.
- Starting to grout before the mix submittal has written acceptance.
What comes after the mix is chosen?
With the grout specified, the volume side of the order is next. The bond beam lintel measurement guide shows the field readings and the per-opening volume arithmetic, the Bond Beam Concrete Calculator runs the same course-based volume for any bond beam run, and the Concrete Quantity Planning Tools and Guides hub lists the related concrete calculators and guides.
Safety and professional scope
Grout selection is not structural design. This page does not design the lintel, size reinforcement, set bearing, or certify code compliance. Follow the governing drawings and specifications, and bring a qualified professional into any decision the spec leaves to engineering judgment. The drawings also set the specified strength; the 2,000 psi floor is a minimum, not a recommendation.
Sources and scope
Mix type, strength, slump, proportion, admixture, and mixing figures come from CMHA TEK 09-04A and the IMI masonry grout technology brief, both read in full on 2026-10-15. The f'm relationship is corroborated by a FORSE masonry specification guide.
- CMHA TEK 09-04A, Grout for Concrete Masonry (accessed 2026-10-15): fine and coarse grout definitions, ASTM C476 compliance, 8 to 11 in. slump, 2,000 psi minimum, Table 1 volume proportions, grout type selection factors, admixture and mixing rules, unit strength method, and the 5,000 psi specified maximum for strength design.
- International Masonry Institute, Technology Brief: Masonry Grout (August 2009; accessed 2026-10-15): aggregate size limits, fine vs coarse selection bands, slump-end guidance by conditions, bulk densities for volume-to-weight conversion, air-entrainment caution at rebar, and self-consolidating grout parameters.
- FORSE, Guidelines for Specifying Concrete Masonry with f'm = 2500 psi (2026; accessed 2026-10-15): corroboration of the TMS 602 grout-strength floor relative to f'm.
Source scope: CMHA and IMI support the grout type, strength, slump, proportion, admixture, and mixing claims used here. The worked proportion check on this page verifies the arithmetic independently against the ASTM C476 boundaries. None of these sources designs the lintel, selects reinforcement, or sets the strength for a specific project.
Review note: Saleem Sial owns the research and editorial record. Source checks, build validation, and rendered QA form the internal publication gate. Waseem Sial, External Reviewer, Engineer, is listed for ongoing external review; no completed review date is claimed.